| 项目 | 指标 | ||
| 型号 | CY-Ce01 | CY-Ce02 | CY-Ce03 |
| 氧化铈(CeO2)(w)% | 99.95 | 99.95 | 99.9 |
| 平均粒径(nm) | 10-30nm | 50-80nm | 1-2um |
| 比表面积 (m2/g) | 50-60 | 30-50 | 10-20 |
| 松装比重(g/cm3) | 1.6 | 1.6 | 1.7 |
| Ln2O3 ≤ | 0.01 | 0.01 | 0.01 |
| Nd2O3+Pr6O11 ≤ | 0.03 | 0.03 | 0.03 |
| Fe2O3 ≤ | 0.01 | 0.01 | 0.01 |
| SiO2 ≤ | 0.02 | 0.02 | 0.02 |
| CaO ≤ | 0.01 | 0.01 | 0.01 |
| Al2O3 ≤ | 0.02 | 0.02 | 0.02 |
| 灼减(1000℃,2Hr) | 0.2 | 0.2 | 0.2 |