产品名称
:氟化镁(别名:二氟化镁)| 型号 | CY-FHM30 |
|---|---|
| 外观 | 浅灰色粉末 |
| 粒径(nm) | 30–50 |
| 比表面积(m²/g) | 100–150 |
用作冶炼金属镁的助溶剂、电解铝的添加剂、光学透镜镀膜材料、钛颜料的涂着剂、阴极射线屏的荧光材料等
用于光学玻璃、陶瓷工业及电子工业
用于制造陶器、玻璃,作为冶炼镁的助溶剂,以及光学仪器镜头和滤光器的涂层、光学透镜的反折射剂和焊接剂
固态电池:氟化镁可作为固态电解质的功能添加剂或界面修饰层材料,有助于降低界面阻抗、控制锂枝晶生长、提高固态电池的循环稳定性和安全性。其在宽电化学窗口下表现稳定,适用于高电压固态电池体系。
样品包装:100 g/袋、500 g/袋 或 1 kg/袋
保持密封,存放于阴凉、干燥处,避免受潮。
Product Name: Magnesium Fluoride (also known as Magnesium Difluoride)
CAS No.: 7783-40-6
| Model | CY-FHM30 |
|---|---|
| Appearance | Light gray powder |
| Particle Size (nm) | 30–50 |
| Specific Surface Area (m²/g) | 100–150 |
Used as a flux in magnesium metal smelting, additive in aluminum electrolysis, coating material for optical lenses, pigment extender for titanium pigments, and fluorescent material for cathode ray screens
Applied in optical glass, ceramic industry, and electronic industry
Used in the manufacture of pottery and glass, as a flux for magnesium smelting, as a coating for lenses and filters in optical instruments, as an anti-refractive agent for optical lenses, and as a soldering agent
Solid-State Batteries: Magnesium fluoride can be used as a functional additive for solid-state electrolytes or as an interfacial modification layer. It helps reduce interfacial resistance, suppress lithium dendrite growth, and enhance the cycling stability and safety of solid-state batteries. With stable performance under a wide electrochemical window, it is suitable for high-voltage solid-state battery systems.
Sample packaging: 100 g/bag, 500 g/bag, or 1 kg/bag
Keep container sealed and store in a cool, dry place away from moisture.